Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer Ineos ABS
Trade Name Lustran®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® 1152.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
Elongation at Break 40 %
40 %
Nominal
Elongation at Yield 3.5 %
3.5 %
Tensile Modulus 1.52 GPa
220 ksi
Charpy Impact, Notched 5.40 J/cm²
25.7 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 104 µm/m-°C

@Temperature 20.0 °C
57.8 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °C
192 °F
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL Recognized
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Injection Molding
Mold Temperature 60.0 °C
140 °F
Injection Molding
Injection Velocity 200 mm/sec
7.87 in/sec
Injection Pressure 55.0 MPa
7980 psi