Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) X 30 S Polypropylene Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) X 30 S Polypropylene Film.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polypropylene film with good optical propertiesApplications: film, packing food stuffs, stationary and textiles.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 9.0 g/10 min
9.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
ISO 868
Tensile Stress 34.0 MPa
4930 psi
ISO R527
Elongation at Yield 13 %
13 %
ISO R527
Flexural Modulus 1.50 GPa
218 ksi
ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ISO 306/A
Heat Distortion Temperature 115 °C
239 °F
ISO 75/B