| Category | Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), Extrusion Grade |
| Manufacturer | Isoflon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Isoflon PEI Polyetherimide.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | DIN 53479 |
| Water Absorption | 0.25 % | 0.25 % | ASTM D570 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 109 | 109 | ASTM D785 |
| Tensile Strength | 105 MPa | 15200 psi | DIN 53455 |
| Elongation at Break | 60 % | 60 % | DIN 53455 |
| Tensile Modulus | 3.10 GPa | 450 ksi | DIN 53457 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 62.0 µm/m-°C | 34.4 µin/in-°F | DIN 52328 |
| Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 215 °C | 419 °F | DIN 53736 |
| Maximum Service Temperature, Air | 170 °C | 338 °F | Continuous; DIN 52612 |
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | |
| Flammability, UL94 | V-0 @Thickness 0.410 mm |
V-0 @Thickness 0.0161 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+17 ohm-cm | 1.00e+17 ohm-cm | DIN 53482 |
| Dielectric Constant | 3.2 @Frequency 1000 Hz |
3.2 @Frequency 1000 Hz |
DIN 53483 |
| Dielectric Strength | 27.0 - 32.0 kV/mm | 686 - 813 kV/in | DIN 53481 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Amber Dark Translucent |