| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Cycoloy® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.13 g/cc | 1.13 g/cc | ASTM D 792 |
| Density | 1.13 g/cc | 0.0408 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.080 % | 0.080 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.30 % @Temperature 23.0 °C |
0.30 % @Temperature 73.4 °F |
ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0090 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0090 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 10 g/10 min @Load 5.00 kg, Temperature 260 °C |
10 g/10 min @Load 11.0 lb, Temperature 500 °F |
[cm^3/10 min] Melt Volume Rate; ISO 1133 |
| 11 g/10 min @Load 5.00 kg, Temperature 260 °C |
11 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D 1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D 638 |
| 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 53.0 MPa | 7690 psi | Type I, 50 mm/min; ASTM D 638 |
| 53.0 MPa | 7690 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 100 % | 100 % | Type I, 50 mm/min; ASTM D 638 |
| 100 % | 100 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 5.0 % | 5.0 % | Type I, 50 mm/min; ASTM D 638 |
| 5.0 % | 5.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.10 GPa | 305 ksi | 1 mm/min; ISO 527 |
| 2.15 GPa | 312 ksi | 5 mm/min; ASTM D 638 | |
| Flexural Yield Strength | 76.0 MPa | 11000 psi | 2 mm/min; ISO 178 |
| 78.0 MPa | 11300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
| 2.10 GPa | 305 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 | |
| Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| 5.20 J/cm @Temperature 23.0 °C |
9.74 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 | |
| Izod Impact, Notched (ISO) | 40.0 kJ/m² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
| 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A | |
| Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 5.50 J/cm² @Temperature 23.0 °C |
26.2 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Impact Test | 60.0 J @Temperature 23.0 °C |
44.3 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 80.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.4 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 127 °C | 261 °F | Rate B/50; ASTM D 1525 |
| 127 °C | 261 °F | Rate B/50; ISO 306 | |
| 128 °C | 262 °F | Rate B/120; ISO 306 |