Material Notes:
Kennametal Stellite'sâ„¢ cobalt base alloys are available as cobalt rods, cobalt electrodes, cobalt wire and cobalt powder.Cobalt alloys are used primarily for wear applications and are particularly well-suited for hardfacing applications.Information provided by Kennametal Stelliteâ„¢
Mechanical Properties Metric English Comments
Hardness, Rockwell C 52 - 62
52 - 62
Component Elements Properties Metric English Comments
Carbon, C 2.55 %
2.55 %
Chromium, Cr 32.5 %
32.5 %
Cobalt, Co >= 40.45 %
>= 40.45 %
as balance
Iron, Fe <= 2.0 %
<= 2.0 %
Molybdenum, Mo <= 1.0 %
<= 1.0 %
Nickel, Ni <= 2.0 %
<= 2.0 %
Other <= 1.0 %
<= 1.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 17.5 %
17.5 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition