| Category | Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified |
| Manufacturer | LG Chemical |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | LG Chemical SI-610 Alphalac Polystyrene.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm | 0.0040 - 0.0080 in/in | ASTM D955 |
| Melt Flow | 6.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 98 | 98 | ASTM D785 |
| Tensile Strength, Yield | 26.5 MPa | 3840 psi | 50 mm/min; ASTM D638 |
| Elongation at Break | 70 % | 70 % | 50 mm/min; ASTM D638 |
| Flexural Yield Strength | 44.2 MPa | 6410 psi | 15 mm/min; ASTM D790 |
| Flexural Modulus | 2.20 GPa | 319 ksi | 15 mm/min; ASTM D790 |
| Izod Impact, Notched | 1.47 J/cm @Thickness 6.35 mm |
2.75 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| 1.76 J/cm @Thickness 3.17 mm |
3.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 81.0 °C @Thickness 12.7 mm |
178 °F @Thickness 0.500 in |
Unannealed; ASTM D648 |
| Vicat Softening Point | 101 °C | 214 °F | 1000 g; ASTM D1525 |
| Flammability, UL94 | HB | HB | 1/16 in |
| HB | HB | 1/8 in | |
| Flame Spread | 34.0 mm/min @Thickness 3.17 mm |
1.34 in/min @Thickness 0.125 in |
FH3 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Arc Resistance | 60 - 120 sec | 60 - 120 sec | UL Rating PLC 6 (60-120 sec) |
| Comparative Tracking Index | 400 - 600 V | 400 - 600 V | UL Rating PLC 1 (400-600 volts) |
| Hot Wire Ignition, HWI | 15 - 30 sec | 15 - 30 sec | UL Rating PLC 3 (15-30 sec) |
| High Amp Arc Ignition, HAI | 60 - 120 arcs | 60 - 120 arcs | UL Rating PLC 1 (60-120 arcs) |
| High Voltage Arc-Tracking Rate, HVTR | 10.0 - 25.4 mm/min | 0.394 - 1.00 in/min | UL Rating PLC 1 (10-25.4 mm/min) |