Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loctite® 3883 Stencil Print Isotropic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Loctite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3883 Stencil Print Isotropic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Electrically Conductive BondersLoctite® Electrically Conductive Adhesives are used in a variety of applications where electrical connectivity is needed, providing a conductive path where traditional methods such as solder, are not practical. Electrically Conductive Adhesives are ideal for attaching temperature sensitive components, or providing electrical interconnections on non-solderable substrates, such as plastic and glass.Loctite offers a complete line of electrically conductive adhesives to meet almost any need including: flexible, heat cure, room temperature cure, screen printable, high adhesion, and rapid cure.Loctite® 3883 Stencil Print Isotropic Epoxy AdhesiveA silk screen or stencil adhesive. Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 3.60 g/cc
0.130 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength >= 6.89 MPa
>= 1000 psi
Aluminum to Aluminum
Thermal Properties Metric English Comments
CTE, linear >= 20.0 µm/m-°C

@Temperature 20.0 °C
>= 11.1 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 48.0 °C
118 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.00050 ohm-cm
<= 0.00050 ohm-cm
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
100ºC
120 - 180 min

@Temperature 60.0 °C
2.00 - 3.00 hour

@Temperature 140 °F
Pot Life 96.0 min

@Temperature 23.0 °C
96.0 min

@Temperature 73.4 °F
Users viewing this material also viewed the following: