| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.08 g/cc | 0.0390 lb/in³ | ASTM D792 |
| Water Absorption | 1.2 % | 1.2 % | ASTM D570 |
| Linear Mold Shrinkage | 0.015 cm/cm | 0.015 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | ASTM D638 |
| Elongation at Break | >= 400 % | >= 400 % | ASTM D638 |
| Flexural Yield Strength | 17.0 MPa | 2470 psi | ASTM D790 |
| Flexural Modulus | 1.25 GPa | 181 ksi | ASTM D790 |
| Izod Impact, Notched | 3.33 J/cm | 6.24 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 209 °C | 408 °F | ASTM D789 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 250 °C | 482 °F | |
| Rear Barrel Temperature | 210 °C | 410 °F | |
| Middle Barrel Temperature | 230 °C | 446 °F | |
| Front Barrel Temperature | 250 °C | 482 °F | |
| Nozzle Temperature | 250 °C | 482 °F | |
| Mold Temperature | 80.0 °C | 176 °F | |
| Drying Temperature | 76.0 °C | 169 °F |