Material Notes:
NYCOA 2084 HS is a high viscosity resin particularly suitable for extrusion processing. Its melt viscosity and strength provide ease of processing for tubing, profile, and molded articles. This material has been specially formulated with an organic heat stabilizer to eliminate copper iodide extraction in windshield-wiper tubing applications. In addition, the base resin in fully extracted to minimize caprolactam extractables. Typical applications include automotive tubing, windshield washer tubing, and hoses.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hours; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Strength 40.0 MPa
5800 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 8.00 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ASTM D789