Material Notes:
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, material handling, step pads and other applications requiring rigid TPOs. This recyclable product is a tough, high-strength thermoplastic that maintains its properties over a wide temperature range.Information provided by Noble Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.01 MPa
2902 psi
ASTM D638
Elongation at Break 185.8 %
185.8 %
ASTM D412
Izod Impact, Notched 4.68 J/cm

@Temperature -30.0 °C
8.77 ft-lb/in

@Temperature -22.0 °F
ASTM D256
6.09 J/cm

@Temperature 23.0 °C
11.4 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact 20.3 J

@Temperature 23.0 °C
15.0 ft-lb

@Temperature 73.4 °F
ASTM D5420
22.64 J

@Temperature -30.0 °C
16.70 ft-lb

@Temperature -22.0 °F
ASTM D5420
Tangent Modulus 1310 MPa
190000 psi
ASTM D790
Processing Properties Metric English Comments
Middle Barrel Temperature 191 - 218 °C
375 - 425 °F
Ejection Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Water Temperature