Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 0.976 g/cc
0.976 g/cc
Viscosity 300 - 900 cP

@Temperature 25.0 °C
300 - 900 cP

@Temperature 77.0 °F
Descriptive Properties Value Comments
Appearance at 25°C Clear Pale Yellow Liquid
Equivalent Weight 463