| Category | Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Encapsulation Grade |
| Manufacturer | Dow Corning |
| Trade Name | SLYGARD® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.990 g/cc @Temperature 25.0 °C |
0.990 g/cc @Temperature 77.0 °F |
|
| Viscosity | 3300 cP | 3300 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 55 | 55 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 730 µm/m-°C | 406 µin/in-°F | |
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 90 % | 90 % | transparent; thickness not quantified |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.10e+15 ohm-cm | 1.10e+15 ohm-cm | |
| Dielectric Constant | 2.85 @Frequency 100 Hz |
2.85 @Frequency 100 Hz |
|
| 2.86 @Frequency 100000 Hz |
2.86 @Frequency 100000 Hz |
||
| Dielectric Strength | 16.3 kV/mm | 415 kV/in | |
| Dissipation Factor | <= 0.00010 @Frequency 100000 Hz |
<= 0.00010 @Frequency 100000 Hz |
|
| 0.0030 @Frequency 100 Hz |
0.0030 @Frequency 100 Hz |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 180 - 1440 min @Temperature 22.0 °C |
3.00 - 24.0 hour @Temperature 71.6 °F |
|
| Shelf Life | 12.0 Month | 12.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | clear | |
| Flowable | yes | |
| Gel Hardness (Grams/Penetration) | 100 | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes | |
| Working Time (min) | 20 |