| Category | Fluid , Lubricant , Perfluoropolyether (PFPE) , PTFE Gellant |
| Manufacturer | Nye Lubricants |
| Trade Name | UniFlor |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Nye Lubricants UniFlor 8921SU (UF) Synthetic Oil.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Viscosity Measurement | 340 | 340 | Viscosity Index of Base Oil; ASTM D2270 |
| Kinematic Viscosity at 40°C (104°F) | 134 cSt | 134 cSt | Base Oil; ASTM D445 |
| Kinematic Viscosity at 100°C (212°F) | 40 cSt | 40 cSt | Base Oil; ASTM D445 |
| Evaporation Loss | 0.00 % | 0.00 % | 24 hrs, 100C; ASTM D972 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 357 | 357 | ASTM D217 |
| Oil Separation | 8.7 % | 8.7 % | 24 hrs, 100C; FTM 719B, 321.2 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 200 °C | 392 °F | Recommended |
| Minimum Service Temperature, Air | -65.0 °C | -85.0 °F | Recommended |
| Pour Point | -70.0 °C | -94.0 °F | Base Oil; ASTM D97 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Base Fluid Type | PFPE(lin) | |
| Gellant Type | PTFE |