Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nylene® PX3422 Nylon 6, Impact Extrusion Grade

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer Nylene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nylene® PX3422 Nylon 6, Impact Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dry as molded. Film Grade. Nylene PX3422 is a heat stabilized, high impact modified nylon resin designed for maximum toughness with minimum sacrifice in tensile strength and melting point. PX3422 offers outstanding elongation and good retention of that elongation after 5 days of heat aging at 177 ºC (95% elongation). Optimum processing conditions should provide a melt temperature of 490 - 530ºF at the die.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 310 %
310 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
ASTM D790
Izod Impact, Notched 8.30 J/cm
15.5 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ASTM D495
Processing Properties Metric English Comments
Processing Temperature 265 °C
509 °F