Material Notes:
High strength, good impact resistant material for mechanical components. Excellent hardenability. High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FC-0208-50HTAll information provided by Pacific Sintered Metals.
Physical Properties Metric English Comments
Density 6.00 - 6.40 g/cc
0.217 - 0.231 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 20
20
Tensile Strength, Ultimate 448 MPa
65000 psi
Tensile Strength, Yield 448 MPa
65000 psi
Elongation at Break <= 1.0 %
<= 1.0 %
Flexural Strength 655 MPa
95000 psi
Transverse Rupture
Charpy Impact, Unnotched 4.07 J
3.00 ft-lb