| Category | Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded |
| Manufacturer | Plaskolite |
| Trade Name | Optix® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Plaskolite Optix® CA-924 Impact Modified Acrylic Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.17 g/cc | 0.0423 lb/in³ | ASTM D792 |
| Melt Flow | 6.3 g/10 min | 6.3 g/10 min | Condition 230/3.8; ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | 58.0 MPa | 8410 psi | ASTM D638 |
| Elongation at Break | 4.6 % | 4.6 % | ASTM D638 |
| Modulus of Elasticity | 3.30 GPa | 479 ksi | ASTM D638 |
| Flexural Strength | 86.0 MPa | 12500 psi | ASTM D790 |
| Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
| Gardner Impact | 1.60 J | 1.18 ft-lb | ASTM D3029 GB |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 83.0 °C | 181 °F | ASTM D648 |
| Vicat Softening Point | 112 °C | 234 °F | ASTM D1525 |
| Flammability, UL94 | HB | HB |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Transmission, Visible | 91.6 % | 91.6 % | Luminous Transmittance, ASTM D1003 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 215 - 249 °C | 419 - 480 °F |