Material Notes:
A Zero Shore Hardness TPE, FlexGel is soft, flexible, and resilient, with excellent chemical and moisture resistance. The material can be decorated, printed, reground, and reprocessed without any significant loss of properties. FlexGel is a controlled viscosity material, formulated with specific properties for specific applications. The material is available in uniform pelletized shape, the natural color being clear to translucent. The material can easily be blended with other materials, including colorants.
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.20 g/cc
1.00 - 1.20 g/cc
Processing Properties Metric English Comments
Processing Temperature 180 - 230 °C
356 - 446 °F
Descriptive Properties Value Comments
Color White