Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen EP401M Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Moplen EP401M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP401M is a block copolymer particularly suitable for injection molding of battery case. Moplen EP401M has a effect on masking the appearance of blush. Moplen EP401M meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. And the components of additives are adequate on the food packaging substances specification of FDA regulation 21 CFR 178.2010.Features: Optimized balance of stiffness and toughness; High impact strength at low temperature; High stiffness; Low warpage; High whitenessApplications: Battery caseInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 9.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 29.4 MPa
4270 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
Izod Impact, Notched 1.47 J/cm
2.76 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525