Material Notes:
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excellent processability, in addition to typical OnFlex™-S properties such as a wide hardness range, low compression set, good colourability and a wide temperature operating range. OnFlex™-S EF compounds are semi-filled, making them opaque and with a medium density.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
ISO 868
Tensile Strength at Break 12.0 MPa
1740 psi
ISO 37
Tensile Stress 4.60 MPa

@Strain 100 %
667 psi

@Strain 100 %
ISO 37
6.00 MPa

@Strain 300 %
870 psi

@Strain 300 %
ISO 37
Elongation at Break 700 %
700 %
ISO 37
Tear Strength 42.0 kN/m
240 pli
ISO 34-1
Abrasion 145
145
[mm³]; DIN 53516
Compression Set 30 %

@Temperature 23.0 °C,
Time 259000 sec
30 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
65 %

@Temperature 70.0 °C,
Time 79200 sec
65 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
91 %

@Temperature 100 °C,
Time 79200 sec
91 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Descriptive Properties Value Comments
Features High Flow
Forms Pellets
Generic Material TPE
Generic Material Type Styrenic Thermoplastic Elastomer (TES)
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Fast
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliances
Automotive Applications
Consumer Applications
General Purpose