| Category | Polymer , Thermoplastic , Elastomer, TPE |
| Manufacturer | Polykemi AB |
| Trade Name | POLYelast |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Polykemi AB POLYelast TPE E706 Thermoplastic Elastomer, EPDM-based.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage | 0.015 - 0.022 cm/cm | 0.015 - 0.022 in/in | With Flow; ISO 2577 |
| 0.015 - 0.022 cm/cm | 0.015 - 0.022 in/in | Across Flow; ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 70 @Time 15.0 sec |
70 @Time 0.00417 hour |
Polykemi |
| Tensile Strength at Break | <= 6.00 MPa | <= 870 psi | ISO/R527 |
| Elongation at Break | 350 % | 350 % | ISO/R527 |
| 100% Modulus | 0.00280 GPa | 0.406 ksi | ISO/R527 |
| 300% Modulus | 0.00380 GPa | 0.551 ksi | ISO/R527 |
| Tear Strength | 27.0 kN/m | 154 pli | D624 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 180 - 205 °C | 356 - 401 °F | |
| Mold Temperature | 40.0 - 60.0 °C | 104 - 140 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Back Pressure | Medium | |
| Holding Pressure () | Low | % of injection pressure |
| Injection Pressure | High | |
| Injection Speed () | Low-Medium |