Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Industries Densetec HDPE Arena Board

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polymer Industries
Trade Name Densetec
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Industries Densetec HDPE Arena Board.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Densetec Arena Board is ideal for hockey rink applications including dasher boards, kick plates and official lines. Densetec Arena Board exhibits the properties of high impact strength, abrasion-resistance, and low coefficient of friction. The material is also moisture, stain and abrasion-resistant. The material’s durability and UV stabilization make it ideally suited for the rigors of harsh hockey rink environments. Densetec Arena Board is available in 1/2”, 3/4” and 1” thicknesses. It is available in 50” x 100” sheet sizes.Information provided by Polymer Industries.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 35 hour
35 hour
CO-630; Condition B; ASTM D1693
45 hour
45 hour
CO-630; Condition A; ASTM D1693
Melt Index of Compound 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break >= 600 %
>= 600 %
2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Brittleness Temperature <= -84.0 °C
<= -119 °F
ASTM D746
Flammability, UL94 HB
HB