Material Notes:
30% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
DIN 53479
Water Absorption 1.2 %
1.2 %
DIN 53495
Linear Mold Shrinkage 0.0016 cm/cm
0.0016 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 130 MPa
18900 psi
ASTM-D638
Elongation at Break 4.0 %
4.0 %
ASTM-D638
Tensile Modulus 7.50 GPa
1090 ksi
ASTM-D790
Flexural Strength 150 MPa
21800 psi
ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
ASTM-D790
Izod Impact, Notched 1.80 J/cm

@Temperature 23.0 °C
3.37 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Melting Point 165 - 175 °C
329 - 347 °F
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in