Material Notes:
Sulphur cured, Ethylene Propylene Rubber, 55-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. ASTM & ISO designation = EPDM.Applications: Excellent water and steam resistance with good compression set properties. Not oil resistant.
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
°IRHD; ASTM D1415
70
70
°IRHD, +10 change after 70 hours @ 100°C; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
-25% change after 70 hours @ 100°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 300 %
300 %
-25% change after 70 hours @ 100°C; ASTM D412
400 %
400 %
ASTM D412
Compression Set 25 %
25 %
22 hours @ 70°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
-40.0 °C
-40.0 °F
Non-brittle after 3 minutes
Flash Point >= 200 °C
>= 392 °F