Material Notes:
Resin cured Ethylene Propylene Terpolymer, 70-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated for applications involving water and steam.Applications: Recommended for use in steam raising plant and heat exchanger equipment. Water and steam resistance is superior to that of Sulphur or Peroxide cured variants. Not suitable for use with mineral or di-ester based lubricants.
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
°IRHD; ASTM D1415
84
84
°IRHD, +10 change after 70 hours @ 150°C; ASTM D1415
Tensile Strength, Yield 10.4 MPa
1510 psi
-20% change after 70 hours @ 150°C; ASTM D412
13.0 MPa
1890 psi
ASTM D412
Elongation at Break 120 %
120 %
-20% change after 70 hours @ 150°C; ASTM D412
150 %
150 %
ASTM D412
Compression Set 15 %
15 %
24 hours @ 150°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Non-brittle after 3 minutes
-30.0 °C
-22.0 °F
Flash Point >= 200 °C
>= 392 °F