Precision Polymer Engineering F70A Fluorosilicone Rubber

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering F70A Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Blue Fluorosilicone Rubber, 60 to 70 °IRHD. Fluorosilicone rubber having methyl, vinyl and fluorine substituent groups on the polymer chain. To meet Aerospace Specification Mil-R-25988B, Class 1, Grade 70.Applications: Excellent heat resistance and low temperature flexibility. Suitable for sealing petroleum oils and hydrocarbon fuels. Fluorosilicones are widely used in aircraft fuel systems.
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
°IRHD; ASTM D1415
70
70
°IRHD, +5 change after 70 hours @ 200°C; ASTM D1415
Tensile Strength, Yield 8.00 MPa
1160 psi
ASTM D412
8.40 MPa
1220 psi
5% change after 70 hours @ 200°C; ASTM D412
Elongation at Break 172 %
172 %
-14% change after 70 hours @ 200°C; ASTM D412
200 %
200 %
ASTM D412
Compression Set 10 %
10 %
22 hours @ 175°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Minimum Service Temperature, Air -57.0 °C
-70.6 °F
TR10
-55.0 °C
-67.0 °F
Flash Point >= 300 °C
>= 572 °F