Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Precision Polymer Engineering V75P Fluoroelastomer Compound

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Precision Polymer Engineering Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Precision Polymer Engineering V75P Fluoroelastomer Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Purple Fluoroelastomer Rubber, 70-80 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out:- M2HK710, A1-10, B38, EF31, EO78, F15, Z1, Z2. Where Z1 = comp-set 30% max, Z2 = purple. ASTM designation = FKM. ISO designation = FPM.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
°IRHD; ASTM D1415
85
85
°IRHD, +10 change after 72 hours @ 250°C; ASTM D1415
Tensile Strength, Yield 7.50 MPa
1090 psi
-25% change after 72 hours @ 250°C; ASTM D412
10.0 MPa
1450 psi
ASTM D412
Elongation at Break 131.25 %
131.25 %
-25% change after 72 hours @ 250°C; ASTM D412
175 %
175 %
ASTM D412
Compression Set 30 %
30 %
24 hours @ 200°C; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Flash Point >= 315 °C
>= 599 °F
Users viewing this material also viewed the following: