Material Notes:
Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accurate and humidity & temperature resistant partsInformation provided by Genistar.
Physical Properties Metric English Comments
Density 1.15 - 1.20 g/cc
0.0415 - 0.0434 lb/in³
Viscosity 150 - 400 cP

@Temperature 30.0 °C
150 - 400 cP

@Temperature 86.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 84 - 85
84 - 85
Tensile Strength at Break 49.0 - 56.0 MPa
7110 - 8120 psi
ASTM D638
Elongation at Break 4.0 - 8.0 %
4.0 - 8.0 %
ASTM D638
Tensile Modulus 3.55 - 3.65 GPa
515 - 529 ksi
ASTM D638
Flexural Strength 80.0 - 85.0 MPa
11600 - 12300 psi
ASTM D790
Flexural Modulus 2.30 - 2.50 GPa
334 - 363 ksi
ASTM D790
Izod Impact, Notched 0.140 - 0.260 J/cm
0.262 - 0.487 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 55.0 - 58.0 °C
131 - 136 °F
ISO 75-2
Descriptive Properties Value Comments
Appearance Translucent