Prodways PLASTCure Model 200 3D Printing Polymer

Category Polymer , Rapid Prototyping Polymer
Manufacturer Prodways
Trade Name PLASTCure
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Prodways PLASTCure Model 200 3D Printing Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High temperature resistance.Thermoforming applicationsInformation provided by Genistar.
Physical Properties Metric English Comments
Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Viscosity 500 - 600 cP

@Temperature 28.0 °C
500 - 600 cP

@Temperature 82.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 81 - 85
81 - 85
Tensile Strength at Break 55.0 - 80.0 MPa
7980 - 11600 psi
ASTM D638
Elongation at Break 0.5 - 1.5 %
0.5 - 1.5 %
ASTM D638
Tensile Modulus 1.90 - 2.00 GPa
276 - 290 ksi
ASTM D638
Flexural Modulus 1.80 - 2.10 GPa
261 - 305 ksi
ASTM D790
Izod Impact, Notched 0.100 - 0.150 J/cm
0.187 - 0.281 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 - 100 °C
194 - 212 °F
ISO 75-2
Descriptive Properties Value Comments
Appearance Hazy orange-skin color