Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet)

Category Polymer , Thermoplastic , Polybenzimidazole (PBI)
Manufacturer Quadrant Engineering Plastics Products
Trade Name Duratron® PBI
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Duratron® PBI CU60 Polybenzimidazole, unfilled, compression molded (ASTM Product Data Sheet).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Duratron® PBI is the highest performance engineering plastic available from Quadrant EPP. It offers the highest mechanical properties of any thermoplastic above 400° F (205° C). Duratron® PBI is ideal for high heat bushings, connectors and valve seats. Duratron® PBI is extremely hard and can offer a challenge to fabricate. Fabrication instructions can be furnished by Quadrant EPP.It offers the highest heat resistance and mechanical property retention over 400°F (205°C) of any unfilled plastic. It has better wear resistance and load carrying capabilities at extreme temperatures than any other reinforced or unreinforced advanced engineering plastic.As an unreinforced material, Duratron® PBI is very "clean" in terms of ionic impurity and it does not outgas (except water). These characteristics make this material very attractive to semiconductor manufacturers for vacuum chamber applications. Duratron® PBI has excellent ultrasonic transparency which makes it an ideal choice for parts such as probe tip lenses in ultrasonic measuring equipment.Duratron® PBI is also an excellent thermal insulator. Other plastics in melt do not stick to PBI. These characteristics make it ideal for contact seals and insulator bushings in plastic production and molding equipment.Data provided by Quadrant Engineering Plastic Products from tests on stock shapes and parts produced by Quadrant EPP. Formerly PBI Performance Products Celazole® PBI. Highest mechanical properties of any plastic above 400°F (204°C) Highest heat deflection temperature 800°F (427°C), with a continuous service capability of 750°F (399°C) in inert environments, or 650°F (343°C) in air with short term exposure potential to 1,000°F (538°C) Lowest coefficient of thermal expansion and highest compressive strength of all unfilled plastics
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.40 %
0.40 %
Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation 5.0 %
5.0 %
Immersion; ASTM D570(2)
Mechanical Properties Metric English Comments
Hardness, Rockwell E 105
105
ASTM D785
Hardness, Rockwell M 125
125
ASTM D785
Hardness, Shore D 94
94
ASTM D2240
Tensile Strength 110 MPa
16000 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 5.86 GPa
850 ksi
ASTM D638
Flexural Strength 221 MPa
32000 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Compressive Strength 345 MPa
50000 psi
10% Def.; ASTM D695
Compressive Modulus 6.21 GPa
900 ksi
ASTM D695
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256 Type A
Coefficient of Friction, Dynamic 0.24
0.24
Dry vs. Steel; QTM55007
K (wear) Factor 121 x 10-8 mm³/N-M
60.0 x 10-10 in³-min/ft-lb-hr
QTM 55010
Limiting Pressure Velocity 1.31 MPa-m/sec
37500 psi-ft/min
4:1 safety factor; QTM 55007
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature -40.0 - 149 °C
13.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.403 W/m-K
2.80 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 316 °C
600 °F
Long Term
Deflection Temperature at 1.8 MPa (264 psi) 427 °C
800 °F
ASTM D648
Glass Transition Temp, Tg 413 °C
775 °F
ASTM D3418
Flammability, UL94 V-0
V-0
1/8 inch (Estimated Rating)
Electrical Properties Metric English Comments
Surface Resistivity per Square >= 1.00e+13 ohm
>= 1.00e+13 ohm
EOS/ESD S11.11
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 21.7 kV/mm
550 kV/in
Short Term; ASTM D149
Dissipation Factor 0.0030

@Frequency 1e+6 Hz
0.0030

@Frequency 1e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
3A-Dairy No
No
Canada AG No
No
FDA No
No
NSF No
No
USDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Unacceptable
Unacceptable
Acids, Weak Limited
Limited
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Acceptable
Acceptable
Conductive / Static Dissipative No
No
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable
Descriptive Properties Value Comments
Machinability 10
1-10, 1=Easier to Machine