Material Notes:
CT 988 is an epoxy-based, paste-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant, low out-gassing polymer system capable of surviving exposure up to 150°C.Applications: Disk drive applications, wire tack, non-acrylic UV bonding.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Cured
Elongation at Break 4.0 %
4.0 %
Cured
Shear Strength 27.6 MPa
4000 psi
Cured, tensile
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Cured
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Cured
Descriptive Properties Value Comments
Color Translucent
Composition Epoxy
Moisture Resistance Excellent
Cured
Peel Shear Strength 2
Toxicity Low
Viscosity Light Paste
At 25°C