Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP PX99848 PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* COLORCOMP* PX99848 is an unfilled Nylon 6 resin.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Moisture Absorption 1.30 %
1.30 %
50% RH, 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break 76.0 MPa
11000 psi
ASTM D638
Tensile Strength, Yield 76.0 MPa
11000 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
ASTM D638
Elongation at Yield 3.5 %
3.5 %
ASTM D638
Tensile Modulus 3.46 GPa
502 ksi
50 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
ASTM D790
Flexural Modulus 2.88 GPa
418 ksi
ASTM D790
Izod Impact, Notched 0.580 J/cm
1.09 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 180 °C

@Thickness 3.20 mm
356 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °C

@Thickness 3.20 mm
135 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: