SABIC Innovative Plastics LNP LUBRICOMP DEL34E PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DEL34E PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 152 MPa
22000 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 2.2 %
2.2 %
Type I, 50 mm/min; ASTM D638
Tensile Modulus 14.0 GPa
2030 ksi
50 mm/min; ASTM D638
Flexural Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 12.5 GPa
1810 ksi
ASTM D790
Izod Impact, Notched 0.860 J/cm
1.61 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.10 J/cm
7.68 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
289 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257