SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics LNP LUBRICOMP WL003 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Lubricomp* WL003 is a compound based on Polybutylene Terephalate resin containing PTFE.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 42.0 MPa
6090 psi
5 mm/min; ISO 527
Elongation at Break 12 %
12 %
5 mm/min; ISO 527
Tensile Modulus 2.40 GPa
348 ksi
1 mm/min; ISO 527
Flexural Yield Strength 71.0 MPa
10300 psi
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C
138 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af