Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DF006 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Thermocomp* DF1006 is a compound based on Polycarbonate resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 129 MPa
18700 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 8.10 GPa
1170 ksi
1 mm/min; ISO 527
Flexural Yield Strength 186 MPa
27000 psi
2 mm/min; ISO 178
Flexural Modulus 6.80 GPa
986 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af