| Category | Polymer , Thermoplastic , Polyetherimide (PEI) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP THERMOCOMP |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP THERMOCOMP EC008APQ PEI.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.44 g/cc | 1.44 g/cc | ASTM D792 |
| Density | 1.433 g/cc | 0.05177 lb/in³ | ASTM D792 |
| Moisture Absorption | 0.110 % | 0.110 % | 50% RH, 24 hrs; ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.00010 - 0.00050 cm/cm @Time 86400 sec |
0.00010 - 0.00050 in/in @Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0010 - 0.0050 cm/cm @Time 86400 sec |
0.0010 - 0.0050 in/in @Time 24.0 hour |
ASTM D955 |
| Melt Flow | 40 g/10 min @Load 6.70 kg, Temperature 380 °C |
40 g/10 min @Load 14.8 lb, Temperature 716 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 112 | 112 | ASTM D785 |
| Tensile Strength at Break | 247 MPa | 35800 psi | 5 mm/min; ISO 527 |
| 268 MPa | 38900 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 0.90 % | 0.90 % | 5 mm/min; ISO 527 |
| 1.0 % | 1.0 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 35.48 GPa | 5146 ksi | 1 mm/min; ISO 527 |
| 39.42 GPa | 5717 ksi | 5 mm/min; ASTM D638 | |
| Flexural Strength | 356 MPa | 51600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 364 MPa | 52800 psi | ISO 178 | |
| Flexural Modulus | 30.56 GPa | 4432 ksi | 2 mm/min; ISO 178 |
| 31.3 GPa | 4540 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Compressive Strength | 218 MPa | 31600 psi | SABIC Method |
| Poissons Ratio | 0.44 | 0.44 | ASTM E 132 |
| Shear Modulus | 4.656 GPa | 675.3 ksi | ASTM C273 |
| Shear Strength | 120 MPa | 17400 psi | ASTM C273 |
| Izod Impact, Notched | 0.640 J/cm | 1.20 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 5.60 J/cm | 10.5 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 6.00 kJ/m² | 2.86 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 33.0 kJ/m² | 15.7 ft-lb/in² | 80*10*4; ISO 180/1U |
| Dart Drop, Total Energy | 7.00 J @Temperature 23.0 °C |
5.16 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 3.00 µm/m-°C @Temperature -40.0 - 150 °C |
1.67 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
| CTE, linear, Transverse to Flow | 40.0 µm/m-°C @Temperature -40.0 - 150 °C |
22.2 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
| Deflection Temperature at 1.8 MPa (264 psi) | 193 °C @Thickness 3.20 mm |
379 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 4100 ohm-cm | 4100 ohm-cm | ASTM D257 |
| Surface Resistance | 450 ohm | 450 ohm | ASTM D257 |