SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MFB71L PP.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* THERMOCOMP* MFB71L is a compound based on Polypropylene resin containing 35% Glass Bead, 5% Glass Fiber. Added features of this material include: Low Extractible.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0070 cm/cm

@Time 86400 sec
0.0070 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.0 MPa
3340 psi
ASTM D638
Elongation at Break 3.3 %
3.3 %
ASTM D638
Tensile Modulus 2.99 GPa
434 ksi
50 mm/min; ASTM D638
Flexural Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 2.95 GPa
428 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.21 J/cm
4.14 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C

@Thickness 3.20 mm
183 °F

@Thickness 0.126 in
unannealed; ASTM D648