Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP THERMOCOMP* RW004 is a compound based on Nylon 66 resin containing Wollastonite.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.0 MPa
11300 psi
ASTM D638
Elongation at Break 3.4 %
3.4 %
ASTM D638
Tensile Modulus 4.96 GPa
719 ksi
50 mm/min; ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 4.75 GPa
689 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm
11.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C

@Thickness 3.20 mm
208 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: