Material Notes:
LNP* THERMOCOMP* WH0500B is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 5.00 g/cc
0.181 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 31.0 MPa
4500 psi
ASTM D 638
Elongation at Break 5.0 %
5.0 %
ASTM D 638
Flexural Strength 62.0 MPa
8990 psi
ASTM D 790
Flexural Modulus 2.17 GPa
315 ksi
ASTM D 790
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 8.01 J/cm

@Temperature 23.0 °C
15.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C

@Thickness 3.20 mm
169 °F

@Thickness 0.126 in
unannealed; ASTM D 648