| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Sulfide (PPS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics NORYL APS430 PPE+PPS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
| Water Absorption | 0.020 % @Time 86400 sec |
0.020 % @Time 24.0 hour |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 122 MPa | 17700 psi | SABIC - Japan Method |
| Elongation at Break | 10 % | 10 % | SABIC - Japan Method |
| Flexural Strength | 166 MPa | 24100 psi | ASTM D790 |
| Flexural Modulus | 8.62 GPa | 1250 ksi | ASTM D790 |
| Izod Impact, Notched | 0.780 J/cm | 1.46 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 18.0 - 58.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
10.0 - 32.2 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
| Deflection Temperature at 0.46 MPa (66 psi) | 255 °C @Thickness 3.20 mm |
491 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
| Flammability, UL94 | V-0 @Thickness 0.800 mm |
V-0 @Thickness 0.0315 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 3.3 @Frequency 50.0 - 60.0 Hz |
3.3 @Frequency 50.0 - 60.0 Hz |
ASTM D150 |