Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF SABIC Innovative Plastics NORYL EM6100 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Medium heat, high impact PPO/HIPS alloy used in the automotive industry.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 70 %
70 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 65.0 MPa
9430 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 4.53 J/cm
8.49 ft-lb/in
ASTM D256
2.24 J/cm

@Temperature -40.0 °C
4.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 211 µm/m-°C

@Temperature -40.0 - 60.0 °C
117 µin/in-°F

@Temperature -40.0 - 140 °F
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 110 °C

@Thickness 6.40 mm
230 °F

@Thickness 0.252 in
unannealed; ASTM D648