| Category | Polymer , Thermoplastic , Fluoropolymer , PVDF |
| Manufacturer | Shanghai Ofluorine |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Shanghai Ofluorine 9201 PVDF Pellets for cables.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.77 - 1.78 g/cc | 1.77 - 1.78 g/cc | ISO R1183D |
| Melt Flow | 4.0 - 8.0 g/10 min <br>@Load 12.5 kg,<br> Temperature 230 °C |
4.0 - 8.0 g/10 min <br>@Load 27.6 lb,<br> Temperature 446 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 68 | 68 | ISO 868 |
| Tensile Strength at Break | >= 26.0 MPa <br>@Strain >=100 % |
>= 3770 psi <br>@Strain >=100 % |
ISO R527 |
| Elongation at Break | >= 100 % | >= 100 % | ISO R527 |
| Flexural Strength | 650 MPa | 94300 psi | ISO 178 |
| Izod Impact, Notched | 8.00 J/cm | 15.0 ft-lb/in | ISO 180 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 141 - 144 °C | 286 - 291 °F | ISO 416C |
| Heat Distortion Temperature | 48.0 °C | 118 °F | ISO 75 |
| Oxygen Index | 43 % | 43 % | ASTM D2863 |