Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Radel® R-7700 Polyphenylsulfone (PPSU)

Category Polymer , Thermoplastic , Polyphenylsulfone (PPSU)
Manufacturer Solvay Specialty Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Radel® R-7700 Polyphenylsulfone (PPSU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Radel® R-7700 polyphenylsulfone sheet was developed specifically for aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, low smoke generation and low toxic gas emissions, thereby complying with the FAA regulation 14CFR Part 25.853 Appendix F. In addition, it has excellent impact resistance and meets typical industry requirements for resistance to aerospace fluids, even under stress.Features: Detergent Resistant; Flame Retardant; Good Processing Stability; Good Toughness; Low Smoke Emission; Low ToxicityUses: Aerospace Applications; Aircraft Applications; Aircraft InteriorsAdditional Properties: Heat Release - Ohio State University (1.52 to 3.18 mm): < 20 kW·min/m²; Heat Release - Ohio State University (1.52 to 3.18 mm): < 55 kW/m²; Smoke Density - ASTM F814 3.0 Ds; Smoke Density - ASTM F814 1.0 Ds; Toxic Gas Emissions - 40 ppm; Toxic Gas Emissions - < 1 ppm; Toxic Gas Emissions - < 2 ppm; Toxic Gas Emissions - < 1 ppm; Toxic Gas Emissions - < 1 ppm; Toxic Gas Emissions - 3 ppmInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.34 - 1.42 g/cc
0.0484 - 0.0513 lb/in³
ASTM D792
Water Absorption 0.35 %

@Time 86400 sec
0.35 %

@Time 24.0 hour
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 58.6 MPa

@Thickness 3.18 mm
8500 psi

@Thickness 0.125 in
ASTM D638
Elongation at Break 15 %

@Thickness 3.18 mm
15 %

@Thickness 0.125 in
ASTM D638
Tensile Modulus 2.28 GPa

@Thickness 3.18 mm
331 ksi

@Thickness 0.125 in
ASTM D638
Flexural Strength 100 MPa

@Thickness 3.18 mm
14500 psi

@Thickness 0.125 in
ASTM D790
Flexural Modulus 2.34 GPa

@Thickness 3.18 mm
339 ksi

@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 1.30 J/cm

@Thickness 3.18 mm
2.44 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.18 mm
NB

@Thickness 0.125 in
ASTM D256
Gardner Impact >= 31.1 J

@Thickness 3.18 mm
>= 22.9 ft-lb

@Thickness 0.125 in
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C

@Thickness 3.20 mm
396 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Agency Ratings AAMA 303; FAA FAR 25.853a; OSU 55/55
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Colors Available
Form Pellets; Sheet
Processing Technique Extrusion; Profile Extrusion
Sheet Extrusion; Thermoforming