| Category | Metal , Nonferrous Metal , Nickel Alloy , Superalloy |
| Manufacturer | Special Metals (includes the former Inco Alloys International Inc.) |
| Trade Name | INCONEL® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Special Metals INCONEL® G-3 Nickel Superalloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.30 g/cc | 0.300 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Ultimate | >= 621 MPa | >= 90000 psi | Min per ASTM B582; Sheet and Plate |
| Tensile Strength, Yield | >= 241 MPa <br>@Strain 0.200 % |
>= 35000 psi <br>@Strain 0.200 % |
Min per ASTM B582; Sheet and Plate |
| Elongation at Break | >= 45 % | >= 45 % | Min per ASTM B582; Sheet and Plate |
| Modulus of Elasticity | 199 GPa | 28900 ksi | in tension |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 14.6 µm/m-°C <br>@Temperature 24.0 - 100 °C |
8.11 µin/in-°F <br>@Temperature 75.2 - 212 °F |
Mean |
| 14.6 µm/m-°C <br>@Temperature 24.0 - 300 °C |
8.11 µin/in-°F <br>@Temperature 75.2 - 572 °F |
Mean | |
| 15.1 µm/m-°C <br>@Temperature 24.0 - 500 °C |
8.39 µin/in-°F <br>@Temperature 75.2 - 932 °F |
Mean | |
| Specific Heat Capacity | 0.453 J/g-°C | 0.108 BTU/lb-°F | |
| Thermal Conductivity | 10.0 W/m-K | 69.4 BTU-in/hr-ft²-°F | |
| Melting Point | 1260 - 1343 °C | 2300 - 2449 °F | |
| Solidus | 1260 °C | 2300 °F | |
| Liquidus | 1343 °C | 2449 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Chromium, Cr | 21 - 23.5 % | 21 - 23.5 % | |
| Copper, Cu | 1.5 - 2.5 % | 1.5 - 2.5 % | |
| Iron, Fe | 18 - 21 % | 18 - 21 % | |
| Molybdenum, Mo | 6.0 - 8.0 % | 6.0 - 8.0 % | |
| Nickel, Ni | 49 % | 49 % | As remainder |