| Category | Metal , Nonferrous Metal , Nickel Alloy , Superalloy |
| Manufacturer | Special Metals (includes the former Inco Alloys International Inc.) |
| Trade Name | INCONEL® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Special Metals INCONEL® HX Nickel Superalloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.22 g/cc | 0.297 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell B | 90 | 90 | Sheet |
| Tensile Strength, Ultimate | 793 MPa | 115000 psi | Sheet |
| Tensile Strength, Yield | 345 MPa @Strain 0.200 % |
50000 psi @Strain 0.200 % |
Sheet |
| Elongation at Break | 45.5 % | 45.5 % | Sheet |
| Modulus of Elasticity | 205 GPa | 29700 ksi | |
| Poissons Ratio | 0.32 | 0.32 | |
| Shear Modulus | 80.0 GPa | 11600 ksi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 13.3 µm/m-°C @Temperature 20.0 - 100 °C |
7.39 µin/in-°F @Temperature 68.0 - 212 °F |
Mean |
| 14.3 µm/m-°C @Temperature 20.0 - 300 °C |
7.94 µin/in-°F @Temperature 68.0 - 572 °F |
Mean | |
| 14.7 µm/m-°C @Temperature 20.0 - 500 °C |
8.17 µin/in-°F @Temperature 68.0 - 932 °F |
Mean | |
| 16.7 µm/m-°C @Temperature 20.0 - 1000 °C |
9.28 µin/in-°F @Temperature 68.0 - 1830 °F |
Mean | |
| Specific Heat Capacity | 0.461 J/g-°C | 0.110 BTU/lb-°F | |
| Thermal Conductivity | 11.6 W/m-K | 80.5 BTU-in/hr-ft²-°F | |
| Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
| Solidus | 1260 °C | 2300 °F | |
| Liquidus | 1355 °C | 2471 °F | |
| Maximum Service Temperature, Air | 1200 °C | 2190 °F | exceptional strength to 1200°C |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.10 % | 0.10 % | |
| Chromium, Cr | 21.8 % | 21.8 % | |
| Cobalt, Co | 1.5 % | 1.5 % | |
| Iron, Fe | 18.5 % | 18.5 % | |
| Manganese, Mn | 0.50 % | 0.50 % | |
| Molybdenum, Mo | 9.0 % | 9.0 % | |
| Nickel, Ni | 47.5 % | 47.5 % | |
| Silicon, Si | 0.50 % | 0.50 % | |
| Tungsten, W | 0.60 % | 0.60 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.000116 ohm-cm | 0.000116 ohm-cm | |
| Magnetic Permeability | 1.01096 | 1.01096 | at 200 Oersted (15.9 kA/m) |
| Magnetic Susceptibility | 0.0000409 | 0.0000409 | Mass Susceptibility at 1000 gauss |