Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Encapsulating, Glass or Mineral Filled , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name Epiall®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Bulk Density 0.900 g/cc
0.0325 lb/in³
ASTM D1895
Density 1.90 g/cc
0.0686 lb/in³
ASTM D792
Water Absorption 0.20 %

@Temperature 50.0 °C,
Time 173000 sec
0.20 %

@Temperature 122 °F,
Time 48.0 hour
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 66
66
ASTM D2583
Tensile Strength at Break 90.0 MPa
13100 psi
ASTM D638
Flexural Strength 150 MPa
21800 psi
at rupture; ASTM D790
Flexural Modulus 16.0 GPa
2320 ksi
ASTM D790
Compressive Strength 240 MPa
34800 psi
ASTM D695
Izod Impact, Notched 0.350 J/cm
0.656 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 16.0 µm/m-°C
8.89 µin/in-°F
ASTM E831
CTE, linear, Transverse to Flow 32.0 µm/m-°C
17.8 µin/in-°F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Post Baked; ASTM D648A
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
wet; ASTM D150
Dielectric Strength 12.9 kV/mm

@Frequency 60.0 Hz
328 kV/in

@Frequency 60.0 Hz
step-by-step, wet; ASTM D149
13.7 kV/mm

@Frequency 60.0 Hz
348 kV/in

@Frequency 60.0 Hz
short time, wet; ASTM D149
Dissipation Factor 0.014

@Frequency 1.00e+6 Hz
0.014

@Frequency 1.00e+6 Hz
wet; ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Descriptive Properties Value Comments
Colors Black, Red, Blue
Form Granular
Molding Method Injection
Transfer