Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
Mooney Viscosity 35 - 65

@Temperature 100 °C
35 - 65

@Temperature 212 °F
ML 1+4
40 - 60

@Temperature 100 °C
40 - 60

@Temperature 212 °F
Standard, ML 1+4
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 90
45 - 90
Tensile Strength, Yield 40.0 MPa
5800 psi
Resilience 40 - 50
40 - 50
Thermal Properties Metric English Comments
Brittleness Temperature -62.0 °C
-79.6 °F
Descriptive Properties Value Comments
Appearance Pale to dark amber solid bale or milled sheets
Health Hazard None
Hydrolytic Stability Very Good
Odor Faint, characteristic
Oil and Fuel Resistance Very Good
Ozone Resistance Excellent
Storage Stability Excellent
Weather Resistance Very Good