| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
| Water Absorption | 0.12 % | 0.12 % | 24 Hrs; ASTM D570 |
| Linear Mold Shrinkage | 0.0070 cm/cm | 0.0070 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 109 | 109 | ASTM D785 |
| Tensile Strength at Break | 48.3 MPa | 7000 psi | ASTM D638 |
| Flexural Strength | 72.4 MPa | 10500 psi | ASTM D790 |
| Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
| Compressive Strength | 62.1 MPa | 9000 psi | ASTM D695 |
| Izod Impact, Notched | 2.14 J/cm | 4.00 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 68.4 µm/m-°C @Temperature 20.0 °C |
38.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 136 °C | 276 °F | ASTM D648 |
| Flammability, UL94 | HB @Thickness 1.59 mm |
HB @Thickness 0.0625 in |