Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techno Polymer Techno ABS LM100 Transparent

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techno Polymer Techno ABS LM100 Transparent.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent shock resistance, rigidity, and processability.Applications: Appliance parts, office and computer equipment, machine parts, and tool handles.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 28 g/10 min

@Load 10.0 kg,
Temperature 220 °C
28 g/10 min

@Load 22.0 lb,
Temperature 428 °F
JIS K7210
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Ultimate 44.1 MPa
6400 psi
50 mm/min; ASTM D638
Flexural Yield Strength 72.6 MPa
10500 psi
15 mm/min. ASTM D790
Flexural Modulus 2.16 GPa
313 ksi
15 mm/min. ASTM D790
Izod Impact, Notched 1.57 J/cm
2.94 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
189 °F
unannealed; ASTM D648
Optical Properties Metric English Comments
Haze 4.0 %
4.0 %
Transmission, Visible 88 %
88 %
Processing Properties Metric English Comments
Processing Temperature 190 - 265 °C
374 - 509 °F
Cylinder temp
Nozzle Temperature 210 - 260 °C
410 - 500 °F
Mold Temperature 45.0 - 60.0 °C
113 - 140 °F
Drying Temperature 80.0 °C
176 °F