Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPC 5720WZ Polypropylene, Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPC 5720WZ Polypropylene, Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very high impact resistance, excellent antistatic properties and has been formulated to allow faster cycling through early demolding.Total Polypropylene 5720WZ has been developed specifically for the injection molding of crates, pails, and other heavy duty articles.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Yield 7.0 %
7.0 %
ASTM D638
Flexural Modulus 1.35 GPa
196 ksi
ASTM D790
Izod Impact, Notched 1.80 J/cm
3.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 - 165 °C
320 - 329 °F
TOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Pressure unspecified; ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Users viewing this material also viewed the following: