| Category | Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP , Polyester Thermoplastic Elastomer |
| Manufacturer | Toyobo |
| Trade Name | Pelprene™ |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Toyobo PELPRENE™ P90B Polyester TPE.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.19 g/cc | 0.0430 lb/in³ | ASTM D792 |
| Moisture Absorption at Equilibrium | 0.40 % | 0.40 % | 23°C, 65% RH |
| Linear Mold Shrinkage | 0.011 cm/cm @Thickness 2.00 mm |
0.011 in/in @Thickness 0.0787 in |
|
| Melt Index of Compound | 20 g/10 min @Temperature 230 °C |
20 g/10 min @Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 96 | 96 | JIS K6301 |
| Hardness, Shore D | 52 | 52 | ASTM D2240 |
| Tensile Strength at Break | 31.0 MPa | 4500 psi | ASTM D638 |
| Elongation at Break | 700 % | 700 % | ASTM D638 |
| 50% Modulus | 0.0147 GPa | 2.13 ksi | ASTM D638 |
| Flexural Modulus | 0.162 GPa | 23.5 ksi | ASTM D790 |
| Compressive Modulus | 0.0133 GPa | 1.93 ksi | 0.1; ASTM D695 |
| Resilience | 65 | 65 | JIS K6301 |
| Izod Impact, Notched | NB | NB | ASTM D256 |
| Tear Strength | 172 kN/m | 981 pli | ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 13 | 13 | ASTM D1044 |
| Compression Set | 57 % | 57 % | JIS K6301 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
| Melting Point | 203 °C | 397 °F | By DSC |
| Maximum Service Temperature, Air | 101 °C | 214 °F | Heat deflection temperature, load unknown; ASTM D648 |
| Vicat Softening Point | 180 °C | 356 °F | ASTM D1525 |
| Brittleness Temperature | <= -65.0 °C | <= -85.0 °F | JIS K6301 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 6.00e+13 ohm-cm | 6.00e+13 ohm-cm | ASTM D257 |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | JIS K2111 |